Flashcard library · Chemistry · PaperFren
Stirring time sets GSH-capped silver nanoparticle size
Glutathione reduces AgNO3 at 60 °C; longer stirring grows spherical Ag nanoparticles from about 3 to 6 nm.
Keep what you just learned
Save these 11 cards to your NoteFren library. Your first review starts right away, and each card links back to the study it came from.
What green reductant/stabilizer was used?
Glutathione (GSH) at 60 °C.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified
At what stirring times were nanoparticles observed?
After 36, 48 and 72 h, with mean size still under 7 nm.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified
Where is the Ag SPR band?
Around 344–354 nm.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified
What crystal structure did XRD show?
Face-centered cubic silver.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified
What TEM diameters correspond to 36/48/72 h?
3.20 ± 0.71, 4.83 ± 1.15 and 6.19 ± 1.59 nm.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified
Which GSH IR bands vanish on Ag binding?
S–H and N–H stretches at 2510, 3331 and 3234 cm−1.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified
When are absorbance peaks absent?
At 1, 3, 6 and 18 h in GSH substrate.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified
What happens to SPR intensity with longer stirring?
It increases gradually until 72 h.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified
What Scherrer sizes were estimated?
About 3–8 nm at 36, 48 and 72 h, matching TEM.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified
What Ag precursor concentration was used?
0.1 M AgNO3, 50 mL, stirred up to 72 h at 60 °C.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified
Why were reductions kept in the dark?
To avoid photochemical side reactions.
Source: Stirring time effect of silver nanoparticles prepared in glutathione mediated by green method · DOI · quote verified