XPS and SIMS map thioglucose SAMs on gold
Thio-glucose binds gold through Au–S; flat films pack better than citrate AuNPs, and ToF-SIMS sees TG–MBP pocket fragments.
Keep what you just learned
Save these 11 cards to your NoteFren library. Your first review starts right away, and each card links back to the study it came from.
What thiol ligand was assembled?
1-β-D-thio-glucose (TG) on Au films and nanoparticles.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified
What S2p energy proves Au–S chemisorption?
Component at about 162 eV.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified
What does the ~164 eV S2p component mean?
Unbound/weakly bound sulfur still on the surface.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified
How much does film C–O intensity rise after TG?
About six-fold at 286.5 eV.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified
What C1s component appears only with MBP?
C2 near 288.5 eV from peptide bonds.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified
How were the AuNPs made?
Microwave Turkevich: HAuCl4 to 97 °C, then citrate, 15 nm target.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified
How much unbound TG remains on NPs after dialysis?
About 30%.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified
What citrate XPS change accompanies TG exchange?
Na 1s falls 22 to 12 at% while Au 4f rises 2 to 6 at%.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified
Which SIMS masses mark TG–MBP pocket complexes?
358 and 375 u.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified
Do NPs match film TG density?
No—lower TG density and weaker MBP interaction on nanoparticles.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified
Overnight TG concentration for films?
0.5 mM TG in 1:1 water/ethanol.
Source: Surface Analysis of Gold Nanoparticles Functionalized with Thiol-Modified Glucose SAMs for Biosensor Applications · DOI · quote verified